Hi,
If your construction Code is ASME pls.follow UCS56.
Thanks & Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282
From: Parveen Kumar Nakwal <pknakwal@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, June 13, 2012 3:33 PM
Subject: [MW:14530] Tolerance of Rate of heating & cooling
Dear Experts.
What is the tolerance limit of Rate of heating and cooling in PWHT process ? Please mention Section & Clause no.
Waiting for reply.
Parveen K. Nakwal
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment