yes u can bore very well but the answer in not so simple.
u can bore with the dimensional restriction of B 16.5
go to the WNRF flanges dimensiontable.
check the length though HUB which is called "Y" in table .
while doing machining from inside the length through HUB dimension ( Y) getting reducing as you increasing the inside diameter.
check the tolerences. if after machining the flange meeting the required height . it will be acceptable otherwise Authorized Inspector will reject the flange .
i was in a same situation 2 months ago . luckily after machining or flange meet the tolerance.
Thanks
Regards
Ansari.
--
Regards
Ansari Intekhab Alam
-- On Mon, Jun 11, 2012 at 4:03 PM, Prasad Ghanekar <prsgne@gmail.com> wrote:
I understand that the flange is ASME B 16.5 WN type.Yes, flange can be bored to suit corresponding pipe schedule.Please see attached code interpretation (B16.5 1996 Interpretations).Regards,PrasadOn Sun, Jun 10, 2012 at 12:05 AM, Aly <mhaskar.aly@gmail.com> wrote:
--
Dear Sir,Please advise,Requirement as per drawing: 3" S160 flange; Supplier has machined the complete bore (ID) of 3"SXXS flange and supplied.Can we use this flange for ASME coded (U stamped) vessels as per ASME SEC VIII-1.If not , kindly provide some Code reference.......Ali Mhaskar
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Regards
Ansari Intekhab Alam
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:
Post a Comment