Dear friend,
If u go for gtaw it will cover min 3mm in pqr... then means u can use the wps upto gtaw 9mm,
Regards
Sankar.k
On Mon, Jun 11, 2012 at 7:02 AM, Parveen Kumar Nakwal <pknakwal@gmail.com> wrote:
Dear Experts,Can we use S.S to S.S 8mm base metal thickness PQR of GTAW (3mm)+SMAW (5mm) for the making for new WPS of S.S to S.S with GTAW only, with 2mm base metal thickness only ?Waiting for reply..Regards.Parveen K. Nakwal--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
shankar
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment