Dear Sir,

 

Here below is Type of Common Material Certificate Based on BS EN 10204

 

Type 2.1: Certificate of Compliance

A document issued by the manufacturer stated that the products are in compliance with the order, without any test result shown.

Type 2.2 Test Report

A document issued by the manufacturer stated that the products are in compliance with the order with test report or test result shown.

Type 3.1 Inspection Certificate

A document issued by the vendor inspection division that independent of the manufacturing department and validated by an authorized inspection representative independent of the manufacturing department.

Type 3.2 Inspection Certificate

A document issued and validated by the manufacturer’s independent and authorized inspection representative with an independent authorized representative of the purchaser and or third party inspector agency validation in accordance with the Specifications of the order.

 

 

The main requirement of 3.2 certificate is all tests to be witnessed and endorsed by third party certifying agency such as BV,GL, LR, DNV, ABI etc.

Type 3.2 certificates shall state:

Name of independent inspection agency

Name of independent inspector who has witnessed the tests

The independent inspector’s identification symbol and signature.

 

Rgds,

 

WN

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Bhavesh.Hansora@dnv.com
Sent: Wednesday, June 20, 2012 10:53 AM
To: materials-welding@googlegroups.com
Subject: [MW:14604] 3.2 certification

 

Dear One,

 

Can I know what is the requirement for 3.2 certification ??

 

Which are the tests to be witness by inspector ?

 

 

Bhavesh Hansora

-----------------------------------

 


************************************************************************************** The contents of this e-mail message and any attachments are confidential and are intended solely for the addressee. If you have received this transmission in error, please immediately notify the sender by return e-mail and delete this message and its attachments. Any unauthorized use, copying or dissemination of this transmission is prohibited. Neither the confidentiality nor the integrity of this message can be vouched for following transmission on the Internet. **************************************************************************************

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...