[MW:14556] Re: USE of PQR of GTAW+SMAW for new WPS GTAW process only.

Dear all,

if you go through 200.4(b) For GTAW, SMAW, GMAW, PAW, and SAW,
or combinations of these processes, a PQR for a process
recording a test coupon that was at least 1⁄2 in. (13 mm) is required
hence u cant creat two WPS.

Regrds,
Mohammed-AI-WI.



On Jun 11, 5:02 am, Parveen Kumar Nakwal <pknak...@gmail.com> wrote:
> Dear Experts,
>
> Can we use S.S to S.S 8mm base metal thickness PQR of GTAW (3mm)+SMAW (5mm)
> for the making for new WPS of S.S to S.S with GTAW only, with 2mm base
> metal thickness only ?
>
> Waiting for reply..
>
> Regards.
> Parveen K. Nakwal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Blog Archive