Re: [MW:14296] ENiCrMo6 - AC operating

Dear Srinivasan,

Yes, the SMAW electrode ENiCrMo-6 is available for welding 9% Nickel steel base material for 
Low temp application with AC. 

You can go for BOHLER brand FOX NIBAS 60/15, which is highly suitable. The catalogue is attached
herewith for your perusal. 


Thanks/Best Regards,

M.Saroj Kumar
Chennai,India.

On Wed, May 16, 2012 at 4:58 PM, Srinivasan Jagannathan <jsrisud@gmail.com> wrote:
Dear Experts,

We have a job to be welded with ENiCrMo6 which operates on DC.

We need to weld with AC current due to Arc Blow / Magnetism.

Is it possible to have SMAW electrode of same specification, operating on AC without compromising Mechanical Properties?

Please advice.

Regards,

Srinivasan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...