Re: [MW:14293] For stainless steel sockets welding purging need or not

socket welding not need purge.
 
George Xue (Xue Guoliang)
Suzhou CXGL Mechanical Engineering Co., Ltd.
China
Tel: +86-512-68639769 Fax: +86-512-68639492
Skype: xuegl2001


2012/5/8 mpk mpk <ranmi2007@gmail.com>
Dear Experts,

For stainless steel sockets welding purging need or not.need reference.

Thank you
MPK.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34874] ASME IX, groove weld during WQT limits for Fillet Weld production

Hi David,  There are two points in WQT. 1. Thickness of Base Metal -T 2. Thickness of Weld Metal -t When you use a combination of two proces...