Based on ASME V must on source side. If no access may put on film side.
Based on logic, source side IQI will represent more accurately
radiation absorption of material being inspected.
Regards
Doni
ASNT MT/PT/RI Level 2
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Based on logic, source side IQI will represent more accurately
radiation absorption of material being inspected.
Regards
Doni
ASNT MT/PT/RI Level 2
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments