-- We are fabricating a SS 316L Fuel Gas scrubber
For PP reasons, an insulation layer has to be applied. The client was asking to apply an anticorrosion coating to the stainless steel material of the vessel for corrosion protection in marine environment.
In our experience we never did that for SS.
What do you think?.
Is there any STD/Code that force that?
Design code: AMSE VIII Div 1
Location: Offshore Plateform
Meilleures salutations
Mokrani Lassaad
EPPM Sa.
00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907
P Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail
This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission
00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907
P Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail
This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments