[MW:14270] RE: 14262] For dissimilar weld CS to SS (pipe)309 L for GTAW process for welding root purging required
Dear Yem Pee
Generally In pipeline welding root purging for CS to SS welding for better penetration & root face fusion is required.
Regards,
jatin
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mpk mpk
Sent: 15 May 2012 AM 08:39
To: materials-welding
Subject: [MW:14262] For dissimilar weld CS to SS (pipe)309 L for GTAW process for welding root purging required
Dear Experts,
For dissimilar weld CS to SS (pipe)309 L for GTAW process for welding root purging required ?
Thank you
Yem Pee
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments