Skip to main content

Re: [MW:13923] Painting before pressure test on pipings - B 31.3

No. there should not be paint application on joints of piping  which are to be Hydro test or Pneumatic test .


Regards,
RK Vichare





----- Original Message -----

From: madhan chozhan

To: materials-welding@googlegroups.com

Sent: Sun, 18 Mar 2012 09:12:16 +0530 (IST)

Subject: [MW:13914] Painting before pressure test on pipings - B 31.3



Gents,
Good day.

I need to know whether leak test (hydro or pneumatic) can be done on piping after painting is done on the welds of pipe line?



ASME B 31.3 says "345.3 Preparation for Leak Test
345.3.1 Joints Exposed. All joints, welds (including
structural attachmentwelds to pressure-containing components),


and bonds shall be left uninsulated and
exposed for examination during leak testing, except that
joints previously tested in accordance with this Code


may be insulated or covered. All joints may be primed
and painted prior to leak testing unless a sensitive leak


test (para. 345.8) is required."

"345.8 Sensitive Leak Test
The test shall be in accordance with the Gas and Bubble
Test method specified in the BPV Code, Section V,


Article 10, or by another method demonstrated to have
equal sensitivity. Sensitivity of the test shall be not less
than 10−3 atm·ml/sec under test conditions.
(a) The test pressure shall be at least the lesser of


105 kPa (15 psi) gage or 25% of the design pressure.
(b) The pressure shall be gradually increased until a
gage pressure the lesser of one-half the test pressure or
170 kPa (25 psi) is attained, at which time a preliminary


check shall be made. Then the pressure shall be gradually
increased in steps until the test pressure is reached,
the pressure being held long enough at each step to
equalize piping strains"



here text in green says it shall be left uncovered expect that joints previously tested in accordance with this code(which test to be done for exception and where it is mentioned on code?) but the text in red says it may be primed and painted which looks controversial, kindly advice me what to follow.















--


To post to this group, send email to materials-welding@googlegroups.com


To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com


For more options, visit this group's bolg at http://materials-welding.blogspot.com/


The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...