Skip to main content

RE: [MW:13908] use of E 7018 -1 & ER 70S-6 to weld SA 516 GR 70 MATERIAL

There is no issue in using the proposed consumables.

 

Only restrict the Manganese content of GTAW wire below 1.6 % to achieve A No. 1 weld metal chemistry.

 

Thanking you,

Rgds,

Prashant

 

 

 

 

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of SK Roy
Sent: Saturday, March 17, 2012 12:33 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13906] use of E 7018 -1 & ER 70S-6 to weld SA 516 GR 70 MATERIAL

 

yes can use



On 17-03-2012 PM 1:53, asad azmi wrote:

Dear All,

 

Vessel is being fabricated as per ASME SEC VIII DIV 1.

 

Base material - SA 516 GR 70 HIC - 30 mm Thk. IMPACT TEST not required.

 

  

normally  we are using E 7018 for SMAW,  ER 70S2 for GTAW  & F7P8 EH12K  for SAW Process to weld  above base material.

 

Can we use E7018-1 for SMAW,  ER 70 S6   for GTAW  & F7P8 EH12K for SAW for the above base material.

 

Please Advice.

 

Thanks & Regards

 

Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--

Sanjeev Kumar Roy
QA/QC Manager

CBL Combustion Systems Pvt. Ltd.
Plot No. 230, Padra-Jambusar Highway
Dabhasa-391 440, District-Vadodara
Gujarat, India

Tel : +91-2662-290381, 290388
Fax : +91-2662-244482


Our new name reflects that we are now 100% owned and operated by our Indian shareholders. While retaining our core values and technologies, the change allows us to further expand our products and services.

(Save Paper, Save Trees, Save Space, Save Money Please do not print this email unless you really need to - Life matters)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Any views or opinions expressed in this email and its attachments are those of the individual sender except where the sender specifically states them to be that of Lamprell.

This E-mail and any attachments are confidential and may also be legally privileged. If you have received this email and any attachments in error, you are on notice of its status. Please (a) notify the sender immediately by reply email; (b) destroy this email and any attachment, and (c) do not use, copy, store and/or disclose to any person this email and any attachments: to do so could be a breach of confidence. Thank you for your co operation. Please contact the Lamprell IT Helpdesk on ithelpdesk@lamprell.com if you need any assistance.

Holding company: Lamprell plc, incorporated in the Isle of Man, registration number 117101C, registered office at Fort Anne, Douglas, Isle of Man IM1 5PD

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...