Hi
-- the minimum spacing between two welds shall be 1.5 times the pipe OD or 5 times the pipe wall thickness whichever is greater.
regards,
madhan
--
On Tue, Mar 6, 2012 at 5:30 PM, murat aksoy <maksoy970@gmail.com> wrote:
Hello my friends,I have a problem.
Is there minimum distance limitation between two weld joints as per ASME B31.3. or ENthanks--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Thanks & Regards
Srirammadhan Piping/painting inspector
Great drill Chaaya
Great Ship
Hamriyah Free zone, UAE
+971-509846269
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments