Skip to main content

RE: [MW:13830] clarification for UT

March 5, 2012

 

Dear Lakshman Kumar,

 

What is the result of your UT experience for thin wall thickness and for which application? Please be specific in your query, and identify exactly the pipe thickness and the type of weld that you are working on.

 

Thanks.

 

PJA

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Lakshman Kumar.B
Sent: Sunday, March 04, 2012 6:57 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:13822] clarification for UT

 

Dear Pablo J Acelajado,

 

What abt for lesser than 6.4 mm, UT didn’t work at their?

 

If so why?(with angle probe and if require we can proceed for 2V skip distance also)

 

Thanks and regards,

Lakshman

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pablo J Acelajado
Sent: Sunday, March 04, 2012 3:14 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:13820] clarification for UT

 

March 4, 2012

 

Dear Lakshman Kumar,

 

UT is very normal for HSAW and LSAW pipe weld testing from 6.4 mm WT up to 31 mm WT. Specification for Line Pipe  ISO 3183:2007 / API 5L 44th edition make use of UT even for lesser than 12 mm WT.

 

Thanks.

 

PJA

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Lakshman Kumar.B
Sent: Sunday, March 04, 2012 11:46 AM
To: materials-welding@googlegroups.com
Subject: [MW:13818] clarification for UT

 

 

 

Dear all,

 

I’m having a doubt about UT.

 

Few of my friend are saying  that UT is not possible for thickness less than 12mm, especially for the weld joints that too pipe line’s is not possible. (or maybe they hope, but practically I had successfully done and doing the same for less thk)

 

I’m having the following queries

1.       Why it is not possible?

2.       Any code / standard is it specified?

3.        Than what is alternate option for lesser thickness NDT(where RT is not possible/feasible due to any safety concern or accessibility)

 

Could any one help us to resolve the queries

Thanks and Regards................?

 

Lakshman Kumar.B|Manager |Lanco Infratech Limited

Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004

Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com

Go Green|The future will thank you

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...