Sohaib
I would be very suspect in this situation. There should be nothing secret about the content of steel plate being used.
At the end of the day, you are paying for the ploate, you should know exactly what you are paying to receive.
Doc...Rockweld
Date: Sat, 3 Mar 2012 13:23:50 -0500
Subject: Re: [MW:13816] Storage Tanks Steel Plates
From: jmejialema@gmail.com
To: materials-welding@googlegroups.com
There is no secret they have to show you the real especification by test or by Mill test Report Certificate from the mill. Your paying. Please see API 650 Standard.
Regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
I would be very suspect in this situation. There should be nothing secret about the content of steel plate being used.
At the end of the day, you are paying for the ploate, you should know exactly what you are paying to receive.
Doc...Rockweld
Date: Sat, 3 Mar 2012 13:23:50 -0500
Subject: Re: [MW:13816] Storage Tanks Steel Plates
From: jmejialema@gmail.com
To: materials-welding@googlegroups.com
There is no secret they have to show you the real especification by test or by Mill test Report Certificate from the mill. Your paying. Please see API 650 Standard.
Regards
jml from Colombia
2012/3/3 SOHAIB GHNAIMAT <sohaib_cegco@yahoo.com>
Gents,
We have an issue with the steel plate manufacturer that he is getting the Raw material in the form of steel slabs from other country, and he is doing the Pre-heating and rolling....etc for the Steel slabs to get the final required steel plates.
Do we require having a mill test certificate for the steel slabs, or is enough to have it for the final steel plates.
The supplier is telling that for the steel slabs all information is secret! Do we need to have the manufacturing process, inspection & test plan for the steel slabs.
He has issued the Inspection & test plan for the processing of steel slabs to final steel plates.
Please advice.
Sohaib
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments