As per K328.4.3 of ASME B31.3 shall be aligned/alignment within the dimensional limits in the welding procedure and the engineering design, except that, no morethan 1.6mm but my problem is no where mentioned in welding procedure or engineering drg about missalignment/off-set of C/S ,L/S But joint of piping. Is anyboth can guaide me on which basis I have to except or reject the joint if it is more than 1.6mm off-set (Thickness of joint is 8 mm,Material specification SA106/B,SA312 SS304 & SS316L- Pipe to Elbo joint/Pipe to pipe joints).
Regards,
RK Vichare
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.