Re: [MW:13426] Straight Face Requirement in Dished End..Reg.,

Dear KCR
 Kindly refer to ASME Sec. VIII Div 1 2010, fig: UW 13.1 (l) and note under the same which reads "When thick is equal to.........."  also look at 2 of page no. 122.  Strictly speaking SF is not required when the thickness of shell and dished end are equal and the joints are made by butt welds. When there is a difference in thickness the 1:3 transition that needs to be made shall  be within the SF.

However, as a good engineering practice the butt weld shall be avoided in the knuckle area.

Gopal




From: kcrtechnical <kcrtechnical@gmail.com>
To: materials-welding@googlegroups.com
Sent: Thursday, 5 January 2012 2:08 PM
Subject: [MW:13413] Straight Face Requirement in Dished End..Reg.,

Dear Friends,
 
Is there any specific requirement specified any PV Codes regarding requirement of Straight Face in Dished Ends.
 
Best regards
K C R
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...