The suitable electrode would be AWS E Ni Cr 4.
Regards,
Manivannan.p
--
MANIVANNAN.P
-- On Mon, Jan 2, 2012 at 11:21 PM, fredric <fredric.prabu@bwgindia.com> wrote:
--Dear Experts
Can some body suggest which Welding electrode to be used for type of casting under ASTM A 560 Gr 50 50 ( UNS R 20500), which has the following constituents
It is primarily 50 Cr 50 Ni, with the following chemistry
Cr - 48 - 52%
Fe - 1% Max
C- 0.1%
Ni balance
Cr+ Ni +Cb should exceed 97.5%
Please advice.
Regards
Fredric Prabu. K
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
MANIVANNAN.P
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments