Hi,
It is not practical to go for 5mm thk. with the weld deposit of 5mm.
You have to go for lesser dimensions.
Thanks,
K.Rajagopal
On Wed, Dec 21, 2011 at 8:15 AM, Sundaram Elumalai <Elumalai.Sundaram@starfab.com.sa> wrote:
--******************************************************************************************Hi,
Now we are qualifying two new PQR for new project for less base metal
thick. (9mm). Code AWS D1.1
ROOT / HOT Pass -GTAW (deposited 4mm)
Fill/Cap - SMAW (deposited 5mm)
We need to perform the impact test as per Client Welding spec for each process.
In this case, we have to go for Sub size with temperature reduction.
Client Welding spec requirement is minimum - 29 °C.
If I go with 10x5mm sub size, I need to reduce 11.1 °C and test to be
done at -40.1°C. ( -29 -11.1)
Then Joule value will considered as per ASTM 370,16 J from the below
second table.
Is it correct ?
With Kind Regards,
S.Elumalai.
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments