Skip to main content

Re: [MW:13216] Tack welder qualification

Dear Sir
Thanks for your guidance.
Still I am not clear with the concept
ASME Sec IX says all welding shall be done by a qualified welder, So
for tacking groove joint,
welder need to be qualified for groove joint.....?
Or if he qualified for fillet joint, he can allowed for tacking groove
joint (Tack either incorporated into the final weld or removed).....?
please reply
Samshuddin.K
Asst Engineer-QSA
N-KOM

On 12/13/11, Morin, Darcy (Bantrel Management Services)
<MorinD@bantrelmanagementservices.com> wrote:
> ASME IX recognizes "Welders and Welding Operators". There is no provision
> for "Tack Welders" in ASME IX. However, ASME B31.3 328.5.1(c) mentions
> "Tack Welders", and here is the subsequent Interpretation of this clause:
>
>
>
> Interpretation 22-35
>
> Subject: ASME B31.3-2008, Para. 328.5.1(c), Tack Welding Welder Performance
> Qualifications
> Date Issued: October 5, 2009
> File: 09-1003
> Question (1): Does ASME B31.3, para. 328.5.1(c) require that tack welds,
> whether they are to
> be incorporated into the final weld or be removed, be made by a qualified
> welder?
> Reply (1): Yes.
> Question (2): Does ASME B31.3, para. 328.5.1(c) require that tack welds be
> made to a qualified
> WPS for that joint?
> Reply (2): Yes; see para. 328.5.1(a).
> Question (3): Does ASME B31.3, para. 328.5.1(c) allow tack welds on a groove
> weld joint to be
> made by a welder qualified on a fillet weld test?
> Reply (3): No. See ASME BPV Code Section IX, para. 303.2.
>
>
> Regards,
>
> Darcy Morin
>
> Bantrel Management Services
> morind@bantrel.com
> o - 780 979 6225
> c - 780 782 5692
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of samshuddin k
> Sent: December 13, 2011 9:49 AM
> To: materials-welding
> Subject: [MW:13203] Tack welder qualification
>
> Dear Experts
> There is any clause in ASME Sec. IX for tack welder qualification.
> Which Code explains tack welder qualification for piping regards
> Samshuddin.K
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> This e-mail and any attachments may contain confidential and
> privileged information. If you are not the intended recipient,
> please notify the sender immediately by return e-mail, delete
> this e-mail and destroy any copies.
>
> Any dissemination or use of this information by a person other
> than the intended recipient is unauthorized and may be illegal.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...