Dear VJ,
As this a non pressure part, U can refer to table 5.8 in AWS D1.1 page 183, 194 as well as you can refer to page 73 notes for additional information.
To define specified fillet size is a minimum leg size as mentioned in page 128 in D1.1
With regards
With regards
Vimal Kumar
+65 9100 2565
Hi Jun
Before measuring the weld size, ensure that the fillet weld is not convex or concave. Dimension fillet welds depends on its weld symbol. See the mark on the left of the weld symbol (triangle). 'Z' is indicating leg length (Z 10 means 10 mm leg length). 'a' is indicating throat thickness (a 7 means 7 mm throat thickness).
Rgds2011/11/11 Jr. Chiong <wichiong@yahoo.com>Experts,How to measure a FILLET WELD SIZE?Eagerly need your valuable response.JunQC Inspector
From: Alpesh Sakhreliya <alpeshsakhreliya@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 11 November 2011, 15:04:45
Subject: Re: [MW:12941] Fillet weld size for Non-pressure part as per sec-VIII Div.2 edition 2010
T X 0.7 = FILLET SIZE--
T= MIN WALL THIK.On Fri, Nov 11, 2011 at 4:37 PM, vaibhav Joshi <vnjoshi.leo@gmail.com> wrote:
Dear Experts, I need an advice on following mentioned case.What should be the fillet size of stiffner attachment weld as per ASME sec-VIII Div-2 ? It is basically a rib welding on non-pressure part but still component is a loading member similar to rib welding in saddle supports.Component : Rib welding to the support structureMaterial : SS304Construction code : ASME sec-VIII Div.2Mentioned the clause no. if possible.Regards,VJ--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--Best Regards,Alpesh SakhreliyaTechnical ServicesGujarat State Petronet LimitedDirect: +91 79 66701527Mobile:+91 9898265772
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments