T X 0.7 = FILLET SIZE
T= MIN WALL THIK.
--
-- T= MIN WALL THIK.
On Fri, Nov 11, 2011 at 4:37 PM, vaibhav Joshi <vnjoshi.leo@gmail.com> wrote:
Dear Experts, I need an advice on following mentioned case.What should be the fillet size of stiffner attachment weld as per ASME sec-VIII Div-2 ? It is basically a rib welding on non-pressure part but still component is a loading member similar to rib welding in saddle supports.Component : Rib welding to the support structureMaterial : SS304Construction code : ASME sec-VIII Div.2Mentioned the clause no. if possible.Regards,VJ--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Best Regards,
Alpesh Sakhreliya
Technical Services
Gujarat State Petronet Limited
Direct: +91 79 66701527
Mobile:+91 9898265772
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments