Hi,
No need to do 2 PQRS. you can do with one PQR to cover required thickness for each process.(Root GTAW and Cover SMAW)
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282

From: MRG <mrgupta_2007@yahoo.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Friday, November 11, 2011 4:41 PM
Subject: [MW:12937] Re: Preparation of WPS and PQR for GTAW and SMAW

Hi Karthik,
Thanks, well noted...so one wps will do but is it necessary to make
two PQR for GTAW and SMAW seprately...Can I show all the information
in one PQR.

RGDS
M R Gupta

On Nov 11, 2:17 pm, Karthik <karthik6...@yahoo.com> wrote:
> Hi,
> If your construction code is ASME,then WPS with Plate or pipe can be used for both in production joint.If there is no Impact test requirements,you can use the WPS with either group number.
> Thanks & Regards,
>
> (Karthik)
>
> Karthikeyan.S
> QA/QC Manager
> Getabec Energy Co.,Ltd.
> 379,Moo6,Soi8,Nikhomphatana,
> Rayong-21180,
> Thailand.
> Phone: 0066 38 897035-8 (Off)
> Fax: 0066 38 897034
> Hand Phone: 0066 892512282
>
> ________________________________
> From: mithailal gupta <mrgupta_2...@yahoo.com>
> To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
> Sent: Friday, November 11, 2011 3:47 PM
> Subject: Re: [MW:12931] Preparation of WPS and PQR for GTAW and SMAW
>
> Dear Vikas
>
> Many thanks for your input....but I am still not sure how to use both the material test specimen together as one is pipe and other is plate material (SA 516 Gr. 70 has different Group no. but P no. is same).
>
> RGDS
> M R Gupta
>
>
> ________________________________
> From: vikas shelke <vikas.shelk...@gmail.com>
> To: materials-welding@googlegroups.com
> Sent: Friday, 11 November 2011 1:28 PM
> Subject: Re: [MW:12928] Preparation of WPS and PQR for GTAW and SMAW
>
> Dear Mr. Gupta,
>
> 1) Only one WPS/PQR can qualify your range.
>
> 2) You can qualify the same using a 20 - 22 mm Plate coupon.
>
> 3) Filler to be used - ER 70S2 & E 7018 for SMAW.
>
> 4) You can qualify with Single -V Butt Joint.
>
> On Fri, Nov 11, 2011 at 9:25 AM, MRG <mrgupta_2...@yahoo.com> wrote:
>
> Dear All
>
>
>
>
>
>
>
> >I have to make a WPS and PQR for Pipe ASTM 106 Gr. B (P no. 1and Gr.
> >no.1) and Dishend SA 516 Gr. 70 (P no. 1 but Gr. no.2) both 40mm thk &
> >24" dia using GTAW Root and Hot Pass then SMAW for the remaining
> >passes as per Sec. IX of ASME.
>
> >Kindly give your input on below points.....
> >1) Is it possible to make only one WPS for the above processes?
> >2) What should be the joint design for both and also SA 516 Gr. 70 is
> >not available in pipe?
> >3) What should be the recommended filler rod and Electrode to be used?
> >4) What thickness of pipe to be used to qualify the above WPS so it
> >can for the production weld?
> >5) What should be the preheat temp and Interpass temp?
>
> >If you have any sample WPS and PQR for this then Pl do forward it to
> >me.
>
> >Looking forward for your reply.
>
> >RGDS
> >M R Gupta
>
> >--
> >To post to this group, send email to materials-welding@googlegroups.com
> >To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> >For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> >The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> --
>
>  Regards,
>
> Vikas Shelke,
>
> +91-9881749268.
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>
> - Show quoted text -

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...