Dear friend,
This material is something like CK30. But this kind of material is heat treatable and you have to sure about this. It is recommended to have a metallographic test on it for undrestanding such a heat treatment.
Regards
On Fri, Nov 4, 2011 at 1:22 PM, U WYNN-NAING <u.wynn-naing@total.com> wrote:
--Dear Experts,
We did PMI test on one unknown machine bolt from crane boom rest and result is as follow:
Can someone tell me how can we trace the steel grade base on this result.
Is there any software available?
Thanks and Rgds,
WN
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66283696
Fax: +98-21-66283693
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments