You may complete the total process in 1 PQR - which will contain all the
details.
Thanks and Regards.................
Lakshman Kumar.B|Manager |Lanco Infratech Limited
Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004
Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com
Go Green|The future will thank you
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of MRG
Sent: Friday, November 11, 2011 3:12 PM
To: Materials & Welding
Subject: [MW:12937] Re: Preparation of WPS and PQR for GTAW and SMAW
Hi Karthik,
Thanks, well noted...so one wps will do but is it necessary to make
two PQR for GTAW and SMAW seprately...Can I show all the information
in one PQR.
RGDS
M R Gupta
On Nov 11, 2:17 pm, Karthik <karthik6...@yahoo.com> wrote:
> Hi,
> If your construction code is ASME,then WPS with Plate or pipe can be used
for both in production joint.If there is no Impact test requirements,you can
use the WPS with either group number.
> Thanks & Regards,
>
> (Karthik)
>
> Karthikeyan.S
> QA/QC Manager
> Getabec Energy Co.,Ltd.
> 379,Moo6,Soi8,Nikhomphatana,
> Rayong-21180,
> Thailand.
> Phone: 0066 38 897035-8 (Off)
> Fax: 0066 38 897034
> Hand Phone: 0066 892512282
>
> ________________________________
> From: mithailal gupta <mrgupta_2...@yahoo.com>
> To: "materials-welding@googlegroups.com"
<materials-welding@googlegroups.com>
> Sent: Friday, November 11, 2011 3:47 PM
> Subject: Re: [MW:12931] Preparation of WPS and PQR for GTAW and SMAW
>
> Dear Vikas
>
> Many thanks for your input....but I am still not sure how to use both the
material test specimen together as one is pipe and other is plate material
(SA 516 Gr. 70 has different Group no. but P no. is same).
>
> RGDS
> M R Gupta
>
>
> ________________________________
> From: vikas shelke <vikas.shelk...@gmail.com>
> To: materials-welding@googlegroups.com
> Sent: Friday, 11 November 2011 1:28 PM
> Subject: Re: [MW:12928] Preparation of WPS and PQR for GTAW and SMAW
>
> Dear Mr. Gupta,
>
> 1) Only one WPS/PQR can qualify your range.
>
> 2) You can qualify the same using a 20 - 22 mm Plate coupon.
>
> 3) Filler to be used - ER 70S2 & E 7018 for SMAW.
>
> 4) You can qualify with Single -V Butt Joint.
>
> On Fri, Nov 11, 2011 at 9:25 AM, MRG <mrgupta_2...@yahoo.com> wrote:
>
> Dear All
>
>
>
>
>
>
>
> >I have to make a WPS and PQR for Pipe ASTM 106 Gr. B (P no. 1and Gr.
> >no.1) and Dishend SA 516 Gr. 70 (P no. 1 but Gr. no.2) both 40mm thk &
> >24" dia using GTAW Root and Hot Pass then SMAW for the remaining
> >passes as per Sec. IX of ASME.
>
> >Kindly give your input on below points.....
> >1) Is it possible to make only one WPS for the above processes?
> >2) What should be the joint design for both and also SA 516 Gr. 70 is
> >not available in pipe?
> >3) What should be the recommended filler rod and Electrode to be used?
> >4) What thickness of pipe to be used to qualify the above WPS so it
> >can for the production weld?
> >5) What should be the preheat temp and Interpass temp?
>
> >If you have any sample WPS and PQR for this then Pl do forward it to
> >me.
>
> >Looking forward for your reply.
>
> >RGDS
> >M R Gupta
>
> >--
> >To post to this group, send email to materials-welding@googlegroups.com
> >To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
> >For more options, visit this group's bolg
athttp://materials-welding.blogspot.com/
> >The views expressed/exchnaged in this group are members personel views
and meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
>
> --
>
> Regards,
>
> Vikas Shelke,
>
> +91-9881749268.
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg
athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg
athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.- Hide quoted text -
>
> - Show quoted text -
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments