I have to make a WPS and PQR for Pipe ASTM 106 Gr. B (P no. 1and Gr.
no.1) and Dishend SA 516 Gr. 70 (P no. 1 but Gr. no.2) both 40mm thk &
24" dia using GTAW Root and Hot Pass then SMAW for the remaining
passes as per Sec. IX of ASME.
Kindly give your input on below points.....
1) Is it possible to make only one WPS for the above processes?
2) What should be the joint design for both and also SA 516 Gr. 70 is
not available in pipe?
3) What should be the recommended filler rod and Electrode to be used?
4) What thickness of pipe to be used to qualify the above WPS so it
can for the production weld?
5) What should be the preheat temp and Interpass temp?
If you have any sample WPS and PQR for this then Pl do forward it to
me.
Looking forward for your reply.
RGDS
M R Gupta
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments