Please give the complete detail of the materials and code being use.
If we use base on ASME code, 19 below no need to apply PWHT.
Ragards,
NUJAKA
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of pradip kumar sil
Sent: Thursday, 10 November, 2011 12:02 AM
To: materials-welding@googlegroups.com
Cc: pgoswami@quickclic.net
Subject: [MW:12906] PWHT requirement of weldolet joint
Dear Sir,
Can anybody tell me how i will calculate PWHT requirement in weldolet joint.
Suppose header pipe thickness is 18 m.m & branch thickness is 8 m.m with
weldolet connection.
Thanks & regards
Pradip
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments