i have a query regarding sr of eco. coils after bending (dia
38.1x38Rx4thk.). the hardness value after bending on compression side
is apprx. 220BHN. inspector is saying that hardness value if exceeds
to160BHN then sr all the bends.
If anybody have info. regarding this plz. share with me.