Hello everyone,
I was wondering where I can find inspection and testing exemptions for
ASME B31.3 piping for O&G flow line piping. I'm not sure, but I think
PHMSA Part 192 talks about pipes operating at less than 20% of SMYS in
class 1 locations, and may be class 2 locations with proper compliance
in welding procedure and welder qualification.
I had a construction foreman ask if line pipes that don't see more
than 500psi can be exempt from some of the three (visual, NDE, and
hydro testing), basically to where they can't do all three if the
pressure is low enough and the class location is 1 or may be 2 with
good design of weld and welder qualfication...
Any advice please?

I understand that B31.3 have different applications compared to B31.4
and B31.8. But I could not find anything anywhere about B31.3, and I
think the information in PHMSA part 192 applies to the pipeline side,
and I was considering applying/adopting it as the closest thing.
Anyway,
Do you have anything that gives a clue for exemption for (B31.4 and
B31.8) inspection, examination, and testing or where one can do x-ray
and not have to worry about hydro or vise versa. Especially for low
pressure welded lines in class 1 locations, and may be some class 2
locations (if possible) as long as all fabrications and fabricators
follow qualified procedures in ASME Section IXAlso for B31.3
Thank you very much.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...