Are there any markings on the head of the bolt or the end of the bolt? If you have marks they can be traced to what it should be.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of U WYNN-NAING
Sent: Friday, November 04, 2011 4:53 AM
To: materials-welding@googlegroups.com
Subject: [MW:12864] Type of steel as per chemical proterties
Dear Experts,
We did PMI test on one unknown machine bolt from crane boom rest and result is as follow:
Can someone tell me how can we trace the steel grade base on this result.
Is there any software available?
Thanks and Rgds,
WN
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Comments