Dear experts
I have a WPS qualified for ASTM A312 TP316L( P No 1, Group No1) with impact test at -70C
So this WPS could cover for material ASTM A312 TP310S( P No1, Group No2) required impact test( the same thickness and diameter)
Thanks alot
Duc, Hoang Van
QC inspector
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
I have a WPS qualified for ASTM A312 TP316L( P No 1, Group No1) with impact test at -70C
So this WPS could cover for material ASTM A312 TP310S( P No1, Group No2) required impact test( the same thickness and diameter)
Thanks alot
Duc, Hoang Van
QC inspector
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments