Re: [MW:12645] use of E 8018 C1 for welding SA 537 CL1 Material

Yes ...You can use E 80 18 -1 or E 7018 -1 for SA 537 CL1 material ...But make sure that there will be impact required or not ?
 
Suresh

On Sun, Oct 9, 2011 at 8:22 PM, asad azmi <azmiasadayub@gmail.com> wrote:
Dear All
 
Greetings.
 
Tank of base material SA 537 CL 1 is being under fabrication as per code API 650.
 
Can we use E 8018 C1 for welding SA 537 CL 1.( thickness 42 mm)
 
Please suggest.
 
Thanks & Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...