What Code you are following ? API 650 , 620 ?
According that code you can find the procedure of bottom tanks welding ....But one thing note that we need to give always low heat Input during welding to minimize the distortion level ...
 
Thanks
Suresh
On Mon, Oct 10, 2011 at 12:03 AM, Ahmed Elgendy <eng.aelgendy@yahoo.com> wrote:
dear sir ....

could  any  one give me the procedure of welding  the bottom of storage tanks.
for gasoline  tanks  diam.  30 mtr circular tank 



best  regards,,,,
eng. a. elgendy



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...