Monday, October 10, 2011

[MW:12649] RE: 12647] Orbital Welding - weld joint preparation

It depends what you have specified in your WPS.

 

  Sincerely;

Patrick Brennan

 

CFM / VR-TESCO LLC

CONTINENTAL FIELD MACHINING

1875 Fox Lane

Elgin, IL, 60123

800.323.1393 Office

847.628.8045 Fax

847.894.3355 Cell

847.628.8026 Direct

www.globalfield.net

pbrennan@globalfield.net                             

 

NOTICE:

The contents of this email and any attachments are confidential and may be privileged.They are intended for the named recipient(s) only.

If this message has been delivered to you in error, please reply to the sender to that effect, don’t forward the message to anyone and delete the message from your computer.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Desai Jignesh (Mumbai - Piping)
Sent: Monday, October 10, 2011 4:06 AM
To: 'materials-welding@googlegroups.com'
Subject: [MW:12647] Orbital Welding - weld joint preparation

 

Is it mandatory to make ‘J’ groove preparation for welding of Piping joints by ORBITAL Welding?

 

Regds/Jignesh


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...