Re: [MW:12434] Measure of Sensitivity on Elliptical Joints of 2"NB pipes or any other Elliptical Radiography Shots.

Thanks my dear sir,

The size of joint is 2"NB Pipe scheduled 40.

Regards,
RK Vichare


---- Original Message -----

From: techno mirza

To: materials-welding@googlegroups.com

Sent: Sat, 10 Sep 2011 12:09:36 +0530 (IST)

Subject: Re: [MW:12402] Measure of Sensitivity on Elliptical Joints of 2"NB pipes or any other Elliptical Radiography Shots.



Dear Mr. RK Vichare,


 


Direct Answer: Preferable wire must cross top & bottom image but, If wires are crossing top image only and meeting the required sensitivity (required wires are appeared) than it should not be rejected (at least not just because of wires are not crossing the bottom image) Provided the gap between two images is less then or equal to 1.5" inch.


Justification to the above mention: Why only top image is very important and not the bottom image?

Because, in elliptical technique Penetrameter should placed on source side and if the top image is meeting the required sensitivity, means the bottom is meeting the required sensitivity for sour because, the distance variation between two images are approximately 2'" inch (I do not know what size in your case)


 


Regards.


Mirza.









From: Ramchandra vichare <vicharerke@indiatimes.com>
To: materials-welding@googlegroups.com
Cc: nms@lntecc.com
Sent: Friday, September 9, 2011 8:55 AM
Subject: [MW:12387] Measure of Sensitivity on Elliptical Joints of 2"NB pipes or any other Elliptical Radiography Shots.

  MOST URGENT PL.


Dear All Experts/Experienced Personal in Process Piping in

Refinery/Radiography /NDT Leverl III (RT),

Dear Friends,

As all related experince personal are know about  Elliptacl Radiography shorts; my question is ; while measureing sensitivity with Wire type penetrameter whether it must be cross top & bottom image of Elliptical coverage area of weld or only top portion of weld.  As per my Field experience I suggested for to cover full Elliptical coverage of weld but one of my vendor is refusing to do this same. In section 5 Artical 2 page 13 Clause(d) confirming IQI Placement for weld- Wire IQI , the IQI(s) shall be place on the weld so that the length of the ire is perpenticular to the length of the weld. I sincerely requested to all experts pl be gauide per return mail.

Mater most urgent & interesting in Radiography technology

With Best Regards,

RK Vichare

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.










--


To post to this group, send email to materials-welding@googlegroups.com


To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com


For more options, visit this group's bolg at http://materials-welding.blogspot.com/


The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...