Hello,

great and interesting question. I believe one solution could be that you do the destructive per heat on the heat o pipes being used for the forming of fittings. 

similarly only 1 fitting (from the heat or lot) may go thru the destructive tests under third part "witness". this shoudl fulfill the condition of 3.2 . Moreover the TPI will be comfortable to mention witness on the IRN

Regards,
Gaurav Podar 

--- On Wed, 7/9/11, Ramprasad Chari <ramprasad.chari@gmail.com> wrote:

From: Ramprasad Chari <ramprasad.chari@gmail.com>
Subject: Re: [MW:12358] 3.2 Certification Query / EN 10204:2004
To: materials-welding@googlegroups.com
Date: Wednesday, 7 September, 2011, 4:00 PM

Since heat is getting tested for various properties under independent agencies,certainly the fittings TC can be endorsed as 3.2 certification.Pipe is a raw material for butt welded fittings which after forming and heat treatment is being confirmed through testing for its compliance to fittings specification like A234GRWPB,A420WPL6,A403 TP316 etc etc.All the key results being witnessed by independent agency by identification and stamping after veryfying the traceability, the endorsement of TC by them converts 3.1 TC to 3.2 TC.
Regards
aarpee

On Wed, Sep 7, 2011 at 11:22 AM, Muni Andy <cmkfc07@gmail.com> wrote:
Dear Mr.Vino,
Required a complete traceability of Base Material Certificate.
Muniyandi.C
DNV
On Tue, Sep 6, 2011 at 8:20 PM, Vino Varghese <vinopvarghese@gmail.com> wrote:

Dear All,

 

We would like to know whether Pipe fittings (Elbow, Tee, Reducer etc…) can be certified to 3.2 Certification from the Base material which is a pipe.(Base material Certificate type is 3.1) and help us by providing what all testing and other requirements to be considered in Inspection Test Plan for Pipe fittings to be endorsed as Type "3.2".

 

Whether physical traceability of base material (in our case, it is carbon steel seamless pipe) at Manufacturer's location is required?

 

NOTE: All mechanical and chemical tests for fittings at an Independent Laboratory shall be done and will be certified by LR, BV etc…. so as to endorse Pipe fittings as "3.2 Certification".

Do we still require a complete traceability of Base Material Certificate; although above test will be done?

 

Please provide your technical guidelines to resolve above query.

 

Hope to see as usual positive response from eveyone.

 

Thanks & Regards

Vino Doha, Qatar

 

 

 

 

 

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...