[MW:12425] Welder Qualification-ASME Sec IX- Clad materials

Gents,
 
I have confused on the above topic, could some one clarify the below situation
 
 
1) 21" ID ,Pipe (AISI 4130 ) cladded by INconel 625 with thickness of 1.5 mm with qualified Welding Procedure in other company.
 
2) We need to overlay the above item 1 , by inconel 625 on the existing Inconel 625
 
3) If i want to qualify the welder, i need to consider the Inconel 625 as base metal or AISI 4130 as base metal ?
 
Pls share your exp, in as this kind of situation

Thanks & regards,

K.Babu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...