Re: [MW:12184] Pressure vessels with external pressure

External pressure can be created 3 ways:

  • From a vacuum inside a vessel and atmospheric pressure outside
  • From a pressure outside a vessel greater than atmospheric (typically from some types of jacket or a surrounding vessel)
  • From a combination of the first two - vacuum inside + pressure greater than atmospheric outside.
Such type of vacuum vessel used in Nuclear field as like in iter.

On Thu, Aug 11, 2011 at 12:48 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear All,
In which plants Pressure vessels with external pressure are used?
Thanx & Regds,
psp 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Regards
Ashish Yadav

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...