PT works on basic principle of Surface tension & contact angle only major play, Gravity force not at all.
Thanks
S.Eswaran
From: khatri ankit <nids01dme011@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 5 August 2011 8:04 PM
Subject: Re: [MW:12118] RE: 12112] Regarding PT & MPI test on overhead position
thank u sir, n may u explain me how the MPI is done in overhead position?
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
On Fri, Aug 5, 2011 at 4:37 PM, Pieper QSI <pieper-qsi@kpnmail.nl> wrote:
You are correct regarding capillary working of PT. But the capillary attraction force of the PT liquid in cracks is greater than the gravitation force therefore you only will face some small gravity problems during application of the liquid, once the fluid is on the surface the natural adhesion and capillary forces will do the job.Met vriendelijke groeten / Best RegardsHerman PieperPieper Quality Support & InspectionPhone: +31 (0)521 380083Fax: +31 (0)84 7539225Cell: +31 (0)6 51691215Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens khatri ankit
Verzonden: vrijdag 5 augustus 2011 12:37
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:12115] RE: 12112] Regarding PT & MPI test on overhead positionbut sir in PT , it works on capillary action, due to overhead position, how it works? may u explain me plz how the penetrant draws in to the discontinuity, there is gravitation force.On Fri, Aug 5, 2011 at 1:18 PM, Pieper QSI <pieper-qsi@kpnmail.nl> wrote:Dear Sir,
You can apply both technologies in the overhead position. There are no
restrictions for these technologies regarding execution position.
Met vriendelijke groeten / Best Regards
Herman Pieper
Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl
-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens khatri ankit
Verzonden: vrijdag 5 augustus 2011 9:25
Aan: Materials & Welding
Onderwerp: [MW:12112] Regarding PT & MPI test on overhead position
Dear Experts,
I just want to know that in overhead position which NDT method is
suitable either DPT or MPI
Kindly mention the significance for the same.
y it's used ? and y it;s not used?
Regards,
Ankit Khatri
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.--To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment