Hi Sandeep,

See the attachments with highlights on 304 S15 steel. The first one for
general description, the composition is not correctly specified. The second
one with the correct specification.
This steel is an austenitic S.S conforming to 304 S.S.

Over the years a lot of BS standards have been replaced with EN standards.
As per the 3rd attachment BS 970 seems to have been replaced by EN 10088.
You may confirm that with the manufacturers.

Thanks.


Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario,Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net


On Sat, Aug 6, 2011 at 4:08 PM, QC TMAK <qc.tmak@technomakfzc.ae> wrote:
> Gents,
>
>
>
> Anybody aware about the below material grade.
>
>
>
>  BS970 304 S15

>
> Thanks & Regards,
>
>
>
> Sandeep.K.P
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...