Hi,
DSS FERRITE CONTENT MEASURING STANDARD IS ASTM E562
FYKI
R Vairamuthu
From: abuhanip@labuanship.com
To: materials-welding@googlegroups.com
Subject: [MW:12098] DUPLEX FERRITE CHECK
Date: Thu, 4 Aug 2011 09:21:07 +0800
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
DSS FERRITE CONTENT MEASURING STANDARD IS ASTM E562
FYKI
R Vairamuthu
From: abuhanip@labuanship.com
To: materials-welding@googlegroups.com
Subject: [MW:12098] DUPLEX FERRITE CHECK
Date: Thu, 4 Aug 2011 09:21:07 +0800
DEAR EXPERTS,
IS IT STATED IN ANY CODE & STANDARD ON HOW MANY POINTS
SHALL WE TAKE FOR DUPLEX FERRITE COUNT?
PLEASE GIVE ME THE SPECIFIC CLAUSE OF CODE & STANDARD IF THERE ARE ANY.
YOUR COMMENT IS REALLY APPRICIATED..
REGARDS,
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments