Re: [MW:12050] change in welding Technique does it require Requalification ?

hi Abdul, QW 401.1 and QW 401.2 are different.
QW 401.1 is specifying about procedure. QW 401.2 is specifying welder ability. When you are preparing welder or review welder certificate or administering of welder, the thing you need is QW-401.2 (not QW-401.1)

Rgds

2011/8/1 Suresh <bobsuresh24@gmail.com>
Dear Abdul ..
 
First you need to mentioned clearly that for what requalification needs? ,Welder perfomance or Procedure Qualification ?
 
Suresh

On Mon, Aug 1, 2011 at 6:11 PM, abdul khan <abdul_khan2010@yahoo.co.in> wrote:
Dear Experts,
 
 
If the welding technique is changed does it require Requalification ? as the QW-401.2  it states.
 
QW-401.2 Essential Variable (Performance).
A change in a welding condition which will affect the ability of a welder to deposit sound weld metal (suchas a change in welding process, deletion of backing, electrode, F-Number, technique, etc.).

 

were as the  QW-401.1 Essential Variable (Procedure). it states Welding technique as Non-Essential variable .

 

Which QW we have to follow  and why ?

 

comments plzzzzzzzzzzzzzzzz.

 

Regards

ABDUL JABBAR KHAN

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday, As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without st...