Monday, August 1, 2011

RE: [MW:12043] FILLET WELD QUALIFICATION BY BUTT WELD AS PER API 1104

Mr. Suresh,

Thanks,

See exact detail below, I hope now it be clear:

 

Position is Fixed, pipe horizontal (like 5G in ASME IX) or

Position is Fixed, pipe Vertical (like 2G in ASME IX)

 

If you could give some reference it will be very helpful to me.

 

Regards,

 

NAJM UL ISLAM

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Suresh
Sent: Sunday, July 31, 2011 4:53 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:12008] FILLET WELD QUALIFICATION BY BUTT WELD AS PER API 1104

 

Mr.Islam ,

 

Your query is not correct ...5G position tells you that pipe is rotating but electrode is constant at 45 degrees

                                        2G position is tells you that pipe should be horizontal  position ..not in vertical ...

 

If the welder is qualified in buttwelds in limited thickness ...welder can qualify for all filletwelds ..unlimited thickness..

 

Thanks

 

Suresh

On Sun, Jul 31, 2011 at 2:09 PM, NAJM UL ISLAM <najmislam246@gmail.com> wrote:

Dear Experts,

Greetings,

 

Can somebody advise me that if a welder is qualified for butt weld either in 5G position (Pipe horizontal) or 2G position (Pipe Vertical) whether  he will be qualified for fillet welds or not.

 

Thanks & Regards

 

NAJM UL ISLAM

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...