Monday, August 1, 2011

Re: [MW:12040] How to prepare WPS and PQR

In  my opinion, it is best to refer API 577 section 6 and appendix C. It describes in details requirement and how to review WPS and PQR.
 
Ahmed Husain
Mob-0547170325



From: Dinesh Somwanshi <som.din@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sat, July 30, 2011 10:24:04 AM
Subject: Re: [MW:11993] How to prepare WPS and PQR

can you tell me you will qualify your wps as per code?
aws d1-1 or asme 9


On Sat, Jul 30, 2011 at 8:35 AM, tahir alam <tahiralam007@gmail.com> wrote:
Hello
Can anybody help me to prepare WPS and PQR of CS plate of thickness 6.3mm and process is SMAW...........pls anybody help me ,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...