Monday, August 1, 2011

Re: [MW:12039] How to prepare WPS and PQR

Dear Tahir,

I can help you send me the following details

Carbon steel - Specification and grade.
Electode - Specification as per AWS.

Details of any trial weld parameters , please make sure that all the parameters listed in the ASME BPV section IX-QW-253 are recorded.


Regards

Rinshad 




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...