Dear friend,
 
You have already PQR for both root and cap. Then u can procced with that PQR for making WPS.
 
Arvinda.

On Sun, Jul 31, 2011 at 3:24 PM, BHARAT GOLE <bharatgole@hotmail.com> wrote:
 I have PQR with for single bevel with E6010 root & E7018 for fill & Cap as per ASME IX
Can I prepare WPS with back weld with help of same PQR.....only using E7018 ?
Expert your comments pl with ref to ASME Clause
Regards
Bharat


 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...