Zakaria,
For this PQR (9mm), thé qualification thickness range with impact test is 9 to 18mm according to QW-403-6 (not 9 to 16mm). When there isn't impact test the qualified thickness range is 1,5 to 18 mm.
Regards
Date: Wed, 11 May 2011 14:41:57 +0000
Subject: [MW:11022] PQR with Impact test, Thick Qualified
From: zakaria.ghrab@gmail.com
To: materials-welding@googlegroups.com
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Date: Wed, 11 May 2011 14:41:57 +0000
Subject: [MW:11022] PQR with Impact test, Thick Qualified
From: zakaria.ghrab@gmail.com
To: materials-welding@googlegroups.com
Hi all,
I have one PQR 9 mm thick, with impact test. The range qualification of qualified WPS with Impact test is 9 mm to 16 mm according QW 403.6 .
My question is; What's the thick range qualification qualified by this PQR without impact test, where it's mention in ASME sect IX ?
Regards
--
I have one PQR 9 mm thick, with impact test. The range qualification of qualified WPS with Impact test is 9 mm to 16 mm according QW 403.6 .
My question is; What's the thick range qualification qualified by this PQR without impact test, where it's mention in ASME sect IX ?
Regards
--
زكرياء غرابGHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment