Hi,

As you seen on drawing we will do fillet weld at this ring.The material grade 42CrMo4 ( SAE 4140 ).
I searched on internet it must be apply preheating which degree nearly 316ᵒ C before welding and after welding it must be apply heat thearetment ( 590  ᵒC-600  ᵒC ) and than cool down at room temperature.
Now i am looking an electrode for this material.
At enclosed i added speciality for this material.Could you advice me an electrode for this material?Which electrode?

Hub.png

--
Saygılarımla.
Best Regards.

Sinan ARSLAN
Mechanical Eng. 
Welding Eng.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34866] Presentation for WPS ,PQR AND WPQ as per ASME Sec IX in power point

Dear Experts.        If anyone having presentation of WPS,PQR and WPQ  as per ASME  SEC.IX  in power point then please share . Regards Sanja...