Wednesday, August 10, 2011

[MW:12177] Welding of ASTM A148 Gr 90-60

Hi Friends

I need to rectify a casting @ 100mm thick with weld buildup @ 100 X 100 X 25mm localised area.

The MOC is ASTM A 148 Gr 90-60 which is a high strength steel casting having UTS: 650 MPa.

Does anyone have any exposure of welding such castings.

Is ASTM A 148 Gr 90-60 a weldable grade and welder friendly ?

What should be the preheat and interpass temp.

Can i get some technical literature on weldability of ASTM A 148 Gr 90-60.

Regards

Prem Nautiyal
Mobile +91- 9004063879 / 9769316004

PREM S NAUTIYAL
CELL : 9769316004

Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:34913] Filler wire

E71T-1C  is Charpy Impact tested at -20degC E71T-1CJ is Charpy impact tested at -40degC. AWS Classification for FCAW is only a supplementary...