Dear Sir,
You can apply both technologies in the overhead position. There are no
restrictions for these technologies regarding execution position.
Met vriendelijke groeten / Best Regards
Herman Pieper
Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl
-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens khatri ankit
Verzonden: vrijdag 5 augustus 2011 9:25
Aan: Materials & Welding
Onderwerp: [MW:12112] Regarding PT & MPI test on overhead position
Dear Experts,
I just want to know that in overhead position which NDT method is
suitable either DPT or MPI
Kindly mention the significance for the same.
y it's used ? and y it;s not used?
Regards,
Ankit Khatri
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
You can apply both technologies in the overhead position. There are no
restrictions for these technologies regarding execution position.
Met vriendelijke groeten / Best Regards
Herman Pieper
Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl
-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens khatri ankit
Verzonden: vrijdag 5 augustus 2011 9:25
Aan: Materials & Welding
Onderwerp: [MW:12112] Regarding PT & MPI test on overhead position
Dear Experts,
I just want to know that in overhead position which NDT method is
suitable either DPT or MPI
Kindly mention the significance for the same.
y it's used ? and y it;s not used?
Regards,
Ankit Khatri
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment